PSM Industries Ferro-TiC® CM High Chrome Tool Steel

Category Ceramic , Carbide , Metal , Ferrous Metal , Tool Steel
Manufacturer PSM Industries
Trade Name Ferro-TiC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Ferro-TiC® CM High Chrome Tool Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ferro-TiC® Steel alloy bonded titanium carbide (TiC) materials are made by advanced powder metallurgy technologies. Unlike tungsten carbide, Ferro-TiC® is bonded by hardenable alloy matrices.For warm metalworking, drawing and forming. Replaces D-2 tool steel. Magnetic.Ferro-TiC® Unique CharacteristicsProvides the lightweight, size, stability, and hardnessVirtually porosity free - significantly better than the A1 ASTM B-276-79 StandardLow specific mass. Ferro-Tic® is 10-20% lighter than its steel counterpart and about 50% lighter than tungsten carbide10 times the wear resistance of tool steelsEconomical fabrication (conventionally machinable in the annealed stage by milling and turning, conventionally heat treatable to achieve high hardness)50-90% less linear size change in heat treat than tool steelsInformation Provided by Ferro-TiC®, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.45 g/cc
0.233 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 48
48
Annealed
69
69
Hardened
Flexural Strength 1280 MPa
185000 psi
Transverse Rupture
Compressive Strength 3320 MPa
482000 psi
Charpy Impact Unnotched 3.692 J/cm²
17.58 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear 5.54 µm/m-°C

@Temperature 21.1 - 524 °C
3.08 µin/in-°F

@Temperature 70.0 - 975 °F
Maximum Service Temperature, Air 524 °C
975 °F
Descriptive Properties Value Comments
Carbide (Vol. %) 45
Linear Size Change Thru Heat Treat % -0.011
Thermal Shock (No. Cycles) 2
Users viewing this material also viewed the following: