Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RH Powdered Metal

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer PSM Industries
Trade Name Pacific Sintered Metals
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RH Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries
Physical Properties Metric English Comments
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 42 - 45
42 - 45
Tensile Strength, Ultimate 276 MPa
40000 psi
Tensile Strength, Yield 152 MPa
22000 psi
Elongation at Break 15 %
15 %
1 in. gauge
Tensile Modulus 79.3 GPa
11500 ksi