Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PSM Industries PolyAlloys MIM-17-4 PH Heat Treated Stainless Steel

Category Metal , Ferrous Metal , Stainless Steel , Precipitation Hardening Stainless
Manufacturer PSM Industries
Trade Name PolyAlloys
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PolyAlloys MIM-17-4 PH Heat Treated Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density 7.60 g/cc
0.275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 40
40
Macro
44
44
Micro
Tensile Strength, Ultimate 1190 MPa
172000 psi
Tensile Strength, Yield 1090 MPa

@Strain 0.200 %
158000 psi

@Strain 0.200 %
Elongation at Break 6.0 %
6.0 %
1 in. gauge
Tensile Modulus 193 GPa
28000 ksi
Descriptive Properties Value Comments
Corrosion Resistance <0.005 g/dm2/day
H<sub>2</sub>SO<sub>4</sub>
Pass
CuSO<sub>4</sub>
Pass
Boil Test (H<sub>2</sub>O)
Users viewing this material also viewed the following: