Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 1 Soft Magnetic Steel

Category Metal , Electronic/Magnetic Alloy
Manufacturer PSM Industries
Trade Name PolyAlloys
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PolyAlloys MIM-Fe-50%Ni Grade 1 Soft Magnetic Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of complexity and near full theoretical density by utilizing Metal Injection Molding (MIM).  MIM can economically produce complex shapes beyond the capability of conventional Powdered Metallurgy.Benefits of Metal Injection Molding96-98% of Theoretical DensityExcellent Mechanical PropertiesAvoids Costly Secondary OperationsExcellent Surface FinishesCapable of Extreme 3-D GeometriesHolds Tight TolerancesExtremely Thin Wall Section CapabilitiesInformation Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 50
50
Macro
Tensile Strength, Ultimate 455 MPa
66000 psi
Tensile Strength, Yield 159 MPa

@Strain 0.200 %
23000 psi

@Strain 0.200 %
Elongation at Yield 30 %
30 %
in 1 in.
Electrical Properties Metric English Comments
Magnetic Permeability >= 40000
>= 40000
47500
47500
Typical
Magnetic Coercive Force, Hc 0.13 Oe
0.13 Oe
Magnetic Remanence, Br 10000 Gauss
10000 Gauss
Descriptive Properties Value Comments
B25 (kG) 13
min
14
Typical
B500 (kG) 15
Users viewing this material also viewed the following: