PSM Industries PolyAlloys MIM-WC-6Co Tungsten Carbide

Category Ceramic , Carbide
Manufacturer PSM Industries
Trade Name PolyAlloys
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PolyAlloys MIM-WC-6Co Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density 15.2 g/cc
0.549 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92.3
92.3
Flexural Strength 3520 MPa
510000 psi
Transverse Rupture