Material Notes:
Mil. T-21014 Class 3, SAE-AMS-T-21014 Class 3, ASTM-B-777-87 Class 3Information Provided by PolyAlloys, a division of PSM Industries
Physical Properties Metric English Comments
Density >= 17.75 g/cc
>= 0.6413 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 29
29
Tensile Strength, Ultimate >= 827 MPa
>= 120000 psi
Tensile Strength, Yield >= 552 MPa

@Strain 0.200 %
>= 80000 psi

@Strain 0.200 %
Elongation at Break >= 6.0 %
>= 6.0 %
1 in. gauge
Tensile Modulus 345 GPa
50000 ksi
Component Elements Properties Metric English Comments
Iron, Fe 1.4 %
1.4 %
Nickel, Ni 3.6 %
3.6 %
Tungsten, W 95 %
95 %