Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 30% Glass Fiber Reinforced
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name Lucet®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS Lucet® GC-225 25% Glass Reinforced Acetal Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.59 g/cc
0.0574 lb/in³
ASTM D792
Water Absorption 0.19 %
0.19 %
24 hours at 73°F; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0090 cm/cm
0.0040 - 0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 98.1 MPa
14200 psi
23°C; 50% RH; ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 196 MPa
28400 psi
23°C; 50% RH; ASTM D570
Flexural Modulus 7.85 GPa
1140 ksi
23°C; 50%RH; ASTM D570
Izod Impact, Notched 0.883 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 0.7937 mm
HB

@Thickness 0.03125 in
UL94
Electrical Properties Metric English Comments
Arc Resistance 125 sec
125 sec
ASTM D495