PTS PBT-15GF 15% Glass Filled PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer Polymer Technology & Services, LLC (PTS)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PTS PBT-15GF 15% Glass Filled PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polymer Technology and Services, LLC (PTS).
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 89.6 MPa

@Thickness 3.17 mm
13000 psi

@Thickness 0.125 in
ASTM D638
Flexural Strength 136.5 MPa
19800 psi
ASTM D790
Flexural Modulus 4.35 GPa
631 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 168.3 °C
335.0 °F
ASTM D648