Pacific Sintered Materials BT-126 Bronze Powdered Metal

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials BT-126 Bronze Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Higher strength structural and bearing bronze.All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.60 - 7.80 g/cc
0.275 - 0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell E 78
78
Tensile Strength, Ultimate 317 MPa
46000 psi
Tensile Strength, Yield 248 MPa
36000 psi
Elongation at Break 6.0 %
6.0 %
Flexural Strength 593 MPa
86000 psi
Transverse Rupture
Charpy Impact, Unnotched 6.78 J
5.00 ft-lb
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000157 ohm-cm
0.0000157 ohm-cm
Descriptive Properties Value Comments
Electrical Conductivity (% IACS) 11