Pacific Sintered Materials BZ-111-UC Yellow Brass Powdered Metal

Category Metal , Nonferrous Metal , Copper Alloy , Brass
Manufacturer Pacific Sintered Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials BZ-111-UC Yellow Brass Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: 80-20 leaded brass, coined for close dimensional control, strength and density.Equivalent MPIF Specification: CZP-2000-12All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.80 - 8.00 g/cc
0.282 - 0.289 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell H 90
90
Tensile Strength, Ultimate 207 MPa
30000 psi
Tensile Strength, Yield 110 MPa
16000 psi
Elongation at Break 14 %
14 %
Flexural Strength 483 MPa
70000 psi
Transverse Rupture
Charpy Impact, Unnotched 75.9 J
56.0 ft-lb
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000639 ohm-cm
0.00000639 ohm-cm
Descriptive Properties Value Comments
Electrical Conductivity (% IACS) 27