Pacific Sintered Materials F-241-S2 Iron Soft Magnetic Powdered Metal

Category Metal , Ferrous Metal
Manufacturer Pacific Sintered Materials
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials F-241-S2 Iron Soft Magnetic Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE IV, CLASS AAll information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.00 - 7.20 g/cc
0.253 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 234 MPa
34000 psi
Elongation at Break 11 %
11 %
Electrical Properties Metric English Comments
Magnetic Permeability <= 5.3
<= 5.3
K-Gauss/Oe
Magnetic Coercive Force, Hc 1.7 Oe
1.7 Oe
Magnetic Saturation Flux Density, Bmax 12600 Gauss
12600 Gauss
Magnetic Induction
Magnetic Remanence, Br 10200 Gauss
10200 Gauss