Material Notes:
Applications:Low stressed mechanical componentsSoft magnetic applicationsEquivalent MPIF Specification: F-0000-20All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.20 - 7.60 g/cc
0.260 - 0.275 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Apparent
Tensile Strength, Ultimate 262 MPa
38000 psi
Tensile Strength, Yield 172 MPa
25000 psi
Elongation at Break 7.0 %
7.0 %
Modulus of Elasticity 145 GPa
21000 ksi
Flexural Strength 655 MPa
95000 psi
Transverse Rupture
Charpy Impact, Unnotched 47.5 J
35.0 ft-lb