Material Notes:
Applications:Highly stressed mechanical componentsGood hardenabilityEquivalent MPIF Specification: F-0008-85(HT)All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.80 - 7.20 g/cc
0.246 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 35
35
Apparent
Tensile Strength, Ultimate 655 MPa
95000 psi
Tensile Strength, Yield 655 MPa
95000 psi
Elongation at Break <= 0.50 %
<= 0.50 %
Modulus of Elasticity 138 GPa
20000 ksi
Flexural Strength 1000 MPa
145000 psi
Transverse Rupture
Charpy Impact, Unnotched 6.78 J
5.00 ft-lb
Users viewing this material also viewed the following: