Material Notes:
Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0200-20All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.80 - 7.20 g/cc
0.246 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell F 75
75
Tensile Strength, Ultimate 241 MPa
35000 psi
Tensile Strength, Yield 172 MPa
25000 psi
Elongation at Break 4.0 %
4.0 %
Modulus of Elasticity 138 GPa
20000 ksi
Flexural Strength 552 MPa
80000 psi
Transverse Rupture
Charpy Impact, Unnotched 27.1 J
20.0 ft-lb