Pacific Sintered Materials FN-251-S Invar Powdered Metal

Category Metal , Superalloy , Iron Base
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials FN-251-S Invar Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Coefficient of thermal expansion equal to glass.All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.00 - 7.20 g/cc
0.253 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 32
32
Tensile Strength, Ultimate 276 MPa
40000 psi
Tensile Strength, Yield 276 MPa
40000 psi
Elongation at Break 12 %
12 %
Modulus of Elasticity 94.5 GPa
13700 ksi
Flexural Strength 641 MPa
93000 psi
Transverse Rupture