Material Notes:
High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.80 - 7.20 g/cc
0.246 - 0.260 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 29
29
Tensile Strength, Ultimate 689 MPa
100000 psi
Tensile Strength, Yield 689 MPa
100000 psi
Elongation at Break <= 0.50 %
<= 0.50 %
Modulus of Elasticity 124 GPa
18000 ksi
Flexural Strength 1140 MPa
165000 psi
Transverse Rupture
Charpy Impact, Unnotched 6.10 J
4.50 ft-lb