Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal

Category Metal , Ferrous Metal
Manufacturer Pacific Sintered Materials
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pacific Sintered Materials FX-226-T Infiltrated Iron Powdered Metal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Machines and plates well. Good in hydraulic applications. Moderate tolerance control.Equivalent MPIF Specification: FX-1000-25All information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.20 - 7.50 g/cc
0.260 - 0.271 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65
65
Tensile Strength, Ultimate 352 MPa
51000 psi
Tensile Strength, Yield 221 MPa
32000 psi
Elongation at Break 7.0 %
7.0 %
Modulus of Elasticity 110 GPa
16000 ksi
Flexural Strength 910 MPa
132000 psi
Transverse Rupture
Charpy Impact, Unnotched 33.9 J
25.0 ft-lb