Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO-LOCK SERIES 12 Anaerobic Thread Locking Compound

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO-LOCK SERIES
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO-LOCK SERIES 12 Anaerobic Thread Locking Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TURBO-LOCK 12 SERIES is a fast curing, medium to high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals, and is good in a chemical environment. Disassembles with heat and hand tools.Applications:Ideal for thread locking heavy duty applications such as bolts used in transmission, construction equipment or railroad assemblies, etc.Ideal for fasteners between ¼" and ¾" (6 to 20 mm) diameters.Lubricated for easy assembly. Prevents loosening and leakage of threaded fasteners. Locks and seals threaded joints-nuts, screws, and studs.Meets 90% of all nut and bolt thread locking applications.Meets military specification: MIL-S-46163Part Numbers for this data: 12-000, 12-001, 12-010, 12-050, 12-250, 12-1000Information provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Brookfield Viscosity 2400 cP
2400 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength >= 10.0 MPa
>= 1450 psi
ISO 10123; Compressive, Steel pins and collars
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 35.0 °C
>= 95.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 180 min
1.00 - 3.00 hour
Functional
1440 min
24.0 hour
Full
19.8 min

@Temperature -55.0 - 150 °C
0.330 hour

@Temperature -67.0 - 302 °F
Handling
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Red
Chemical Resistance 100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
85% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
85% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
95% Initial Strength Retained
Acetone at 22°C, at 1000hrs
95% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
95% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
95% Initial Strength Retained
Acetone at 22°C, at 500hrs
95% Initial Strength Retained
Ethanol at 22°C, at 500hrs
95% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
Composition Methacrylate Ester
Max Screw Size 3/4” / 20 mm
Torque 22 N.m
Breakaway, M10 steel nuts and bolts N.m, ISO 10964
32 N.m
Prevail, M10 steel nuts and bolts N.m, ISO 10964
38 N.m
Breakloose, pre-torqued to 5 N.m, M10 steel nuts and bolts, ISO 10964
40 N.m
Max Prevail, pre-torqued to 5 N.m, M10 steel nuts and bolts N.m, ISO 10964
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved