Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO-LOCK SERIES 13 Anaerobic Thread Locking Compound

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO-LOCK SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO-LOCK SERIES 13 Anaerobic Thread Locking Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TURBO-LOCK 13 SERIES is a RED, high temperature, high strength, permanent, anaerobic thread-locking compound. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Disassembles with high heat and hand tools.Applications:Ideal for applications where the temperatures range from -65 to 450ºF.Ideal for thread locking heavy duty applications such as bolts up to 1 ½” (36 mm) used in transmission, construction equipment or railroad assemblies, etc.Lubricated for easy assembly. Prevents loosening and leakage of threaded fasteners. Locks and seals threaded joints-nuts, screws, and studs. To disassemble, apply high heat and use tools.Part Numbers for this data: 13-000, 13-001, 13-010, 13-050, 13-250, 13-1000Information provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Brookfield Viscosity 9500 cP
9500 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength >= 14.5 MPa
>= 2100 psi
ISO 10123; Compressive, Steel pins and collars
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 33.9 °C
>= 93.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 - 180 min
1.00 - 3.00 hour
Functional
1440 min
24.0 hour
Full
30.0 min

@Temperature -55.0 - 204 °C
0.500 hour

@Temperature -67.0 - 399 °F
Handling
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Red
Chemical Resistance 100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 500hrs
100% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
100% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
85% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
90% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
95% Initial Strength Retained
Acetone at 22°C, at 1000hrs
95% Initial Strength Retained
Acetone at 22°C, at 500hrs
95% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
95% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
Composition Methacrylate Ester
Max Screw Size 1 1/2“ / 36 mm
Torque 23 N.m
Breakaway, M10 steel nuts and bolts N.m, ISO 10964
25 N.m
Prevail, M10 steel nuts and bolts N.m, ISO 10964