Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO SEAL SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO SEAL SERIES 75 WHITE GENERAL PURPOSE THREAD SEALANT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TURBO SEAL SERIES 75 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings with lubricating properties to facilitate proper assembly of torque tightening of piping components. It is ideal to seal against gases, water, LPG, hydrocarbons, oils and other chemicals and prevents pipe joints and fittings from loosening and leakage under vibration and shock.Applications:General purpose thread sealant for a wide variety of industrial applications.Typical applications include, metal and fiber plants paper processing plants, chemical processing plants, waste treatment facilities, textile equipment and processing.Part Numbers for this data: 75-050, 75-250Information provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Brookfield Viscosity 90500 cP
90500 cP
RVT Spindle 3 @ 20 rpm
Mechanical Properties Metric English Comments
Shear Strength >= 1.00 MPa
>= 145 psi
Steel Pins & Collars; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 0.800 µm/m-°C
0.444 µin/in-°F
ASTM D696
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Flash Point >= 37.8 °C
>= 100 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min
2.00 - 4.00 hour
Functional
1440 min
24.0 hour
Full
10.0 - 30.0 min

@Temperature -65.0 - 300 °C
0.167 - 0.500 hour

@Temperature -85.0 - 572 °F
Handling
Descriptive Properties Value Comments
Appearance White
Chemical Resistance 100% Initial Strength Retained
Ethanol at 22°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 500hrs
100% Initial Strength Retained
Gasoline at 22°C, at 500hrs
100% Initial Strength Retained
Brake Fluid at 22°C, at 500hrs
100% Initial Strength Retained
Water/Glycol at 87°C, at 500hrs
100% Initial Strength Retained
Motor Oil at 125°C, at 1000hrs
85% Initial Strength Retained
Acetone at 22°C, at 1000hrs
90% Initial Strength Retained
Ethanol at 22°C, at 1000hrs
90% Initial Strength Retained
Brake Fluid at 22°C, at 1000hrs
90% Initial Strength Retained
Water/Glycol at 87°C, at 1000hrs
90% Initial Strength Retained
Acetone at 22°C, at 500hrs
95% Initial Strength Retained
Gasoline at 22°C, at 1000hrs
Composition Methacrylate ester
Torque 1 N.m
Breakaway, M10 steel nuts and bolts, ISO 10964
1 N.m
Prevail, M10 steel nuts and bolts, ISO 10964
23.8 N.m
Max Prevail, pre-torqued to 5 N.m, M10 steel nuts and bolts N.m, ISO 10964
34 N.m
Breakloose, pre-torqued to 5 N.m, M10 steel nuts and bolts, ISO 10964