Material Notes:
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospace applications. Key Features and Benefits:Excellent retention of mechanical properties after long-term high temperature exposureSoft tack and drape propertiesLong ambient out-time for maximum process flexibilityGood electrical properties for RF applicationsMeets requirements of MIL-R-9300B Type IIApplications/Qualifications:Secondary Aircraft StructuresRadomesNacellesInlet DuctsFairingsMeets SS9578 and GMS4001 specifications.Information provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Volatiles <= 2.0 %

@Temperature 163 °C
<= 2.0 %

@Temperature 325 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 379 MPa

@Temperature 138 °C
55000 psi

@Temperature 280 °F
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638
414 MPa

@Temperature 216 °C
60000 psi

@Temperature 420 °F
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638
414 MPa

@Temperature 260 °C
60000 psi

@Temperature 500 °F
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638
448 MPa

@Temperature 177 °C
65000 psi

@Temperature 350 °F
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638
483 MPa

@Temperature 23.9 °C
70000 psi

@Temperature 75.0 °F
0° Direction, Dry, Autoclave with Post-Cure; ASTM D638
Flexural Strength 207 MPa

@Temperature 260 °C
30000 psi

@Temperature 500 °F
Dry, Autoclave with Post-Cure; ASTM D790
276 MPa

@Temperature 216 °C
40000 psi

@Temperature 420 °F
Dry, Autoclave with Post-Cure; ASTM D790
345 MPa

@Temperature 177 °C
50000 psi

@Temperature 350 °F
Dry, Autoclave with Post-Cure; ASTM D790
517 MPa

@Temperature 138 °C
75000 psi

@Temperature 280 °F
Dry, Autoclave with Post-Cure; ASTM D790
586 MPa

@Temperature 23.9 °C
85000 psi

@Temperature 75.0 °F
Dry, Autoclave with Post-Cure; ASTM D790
Compressive Strength 172 MPa

@Temperature 260 °C
25000 psi

@Temperature 500 °F
Dry, Autoclave with Post-Cure; ASTM D695
207 MPa

@Temperature 216 °C
30000 psi

@Temperature 420 °F
Dry, Autoclave with Post-Cure; ASTM D695
345 MPa

@Temperature 177 °C
50000 psi

@Temperature 350 °F
Dry, Autoclave with Post-Cure; ASTM D695
379 MPa

@Temperature 138 °C
55000 psi

@Temperature 280 °F
Dry, Autoclave with Post-Cure; ASTM D695
414 MPa

@Temperature 23.9 °C
60000 psi

@Temperature 75.0 °F
Dry, Autoclave with Post-Cure; ASTM D695
Shear Strength 31.0 MPa

@Temperature 177 °C
4500 psi

@Temperature 350 °F
Short-Beam, Dry, Autoclave with Post-Cure; ASTM D2344
44.8 MPa

@Temperature 23.9 °C
6500 psi

@Temperature 75.0 °F
Short-Beam, Dry, Autoclave with Post-Cure; ASTM D2344
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 180 °C
356 °F
Laminate; standard cure
230 °C
446 °F
Laminate; post cure
Electrical Properties Metric English Comments
Dielectric Constant 3.3 - 3.6

@Frequency 9.375e+9 Hz
3.3 - 3.6

@Frequency 9.375e+9 Hz
Dissipation Factor 0.012 - 0.014

@Frequency 9.375e+9 Hz
0.012 - 0.014

@Frequency 9.375e+9 Hz
Processing Properties Metric English Comments
Gel Time 1.00 - 3.00 min
1.00 - 3.00 min
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Fabric Area Weight (g/m²) 292
Prepreg Resin Content (%) 34-40
Resin Flow (%) 7-21
325°F, 50psi