Parker Chomerics CHO-BOND 1011, Part B

Category Polymer , Adhesive , Thermoset
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1011, Part B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Solubility in Water 0.00 %
0.00 %
Insoluble
Thermal Properties Metric English Comments
Flash Point >= 235 °C
>= 455 °F
Descriptive Properties Value Comments
Dibutyltin dilaurate 77-58-7 Wt. % 100
Physical Form Yellow Liquid, mild odor