Parker Chomerics CHO-FLEX 4408 Conductive Ink

Category Polymer , Thermoset , Polyester, TS
Manufacturer Parker Chomerics
Trade Name CHO-FLEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-FLEX 4408 Conductive Ink.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive InkInformation provided by Chomerics
Physical Properties Metric English Comments
Carbon Black Loading <= 15 %
<= 15 %
Descriptive Properties Value Comments
Color Black
Epoxy Resin, wt % < 40
gamma-Butyrolactone wt. % Max 10
Propylene glycol methyl wt. % 40 - 50