Parker Chomerics CHO-FORM 5532 EMI Shielding Material

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-FORM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-FORM 5532 EMI Shielding Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One component, moisture cure, form-in-place EMI gasketing material. This electrically conductive formulation contains silver-plated copper particles dispersed in a silicone elastomer. Cho-Form® 5531 is designed to be robotically dispensed using high pressure dispense equipmentInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.02 g/cc
3.02 g/cc
2.80 - 3.30 g/cc
2.80 - 3.30 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 26
26
Typical Value; ASTM D2240
<= 45
<= 45
ASTM D2240
Tensile Strength at Break >= 0.414 MPa
>= 60.0 psi
ASTM D412
0.586 MPa
85.0 psi
Typical Value; ASTM D412
Compression Set 30 %
30 %
ASTM D395 Method B 22 hrs 85°C
20 - 45 %
20 - 45 %
ASTM D395 Method B 22 hrs 85°C
Electrical Properties Metric English Comments
Volume Resistivity 0.020 ohm-cm
0.020 ohm-cm
Initial; Chomerics MAT-1002
<= 0.020 ohm-cm
<= 0.020 ohm-cm
Aged; Chomerics MAT-1002
Shielding Effectiveness >= 70 dB
>= 70 dB
Chomerics TP08
Processing Properties Metric English Comments
Extrusion Rate 5.50 - 7.50 g/min
5.50 - 7.50 g/min
Cure Time 2.00 min

@Temperature 65.0 °C
0.0333 hour

@Temperature 149 °F
85% RH
3.00 min

@Temperature 30.0 °C
0.0500 hour

@Temperature 86.0 °F
85% RH
Descriptive Properties Value Comments
Filler Ag/Cu
Resin One Part Silicone
Shear Adhesion N/cm VMin 12