Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield

Category Other Engineering Material
Manufacturer Parker Chomerics
Trade Name CHO-JAC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated emissions limits as well as EU and MIL-STD radiated emissions and susceptibility limits.Information provided by Chomerics
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Polyester Film
35.6 microns
1.40 mil
Copper Foil
88.9 microns
3.50 mil
Total; ASTM D1000
Mechanical Properties Metric English Comments
Tear Strength, Total 11.12 N
2.500 lb (f)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Shielding Effectiveness -100 dB

@Frequency 600 Hz
-100 dB

@Frequency 600 Hz
-10.0 dB

@Frequency 140 Hz
-10.0 dB

@Frequency 140 Hz
-7.00 dB

@Frequency 230 Hz
-7.00 dB

@Frequency 230 Hz
-5.00 dB

@Frequency 200 Hz
-5.00 dB

@Frequency 200 Hz
5.0 dB

@Frequency 400 Hz
5.0 dB

@Frequency 400 Hz
5.0 dB

@Frequency 100 Hz
5.0 dB

@Frequency 100 Hz
12 dB

@Frequency 900 Hz
12 dB

@Frequency 900 Hz
25 dB

@Frequency 40.0 Hz
25 dB

@Frequency 40.0 Hz
50 dB

@Frequency 1.00e+9 Hz
50 dB

@Frequency 1.00e+9 Hz
With 360° ground termination
55 dB

@Frequency 4.00e+8 Hz
55 dB

@Frequency 4.00e+8 Hz
With 360° ground termination
73 dB

@Frequency 1.00e+8 Hz
73 dB

@Frequency 1.00e+8 Hz
With 360° ground termination
75 dB

@Frequency 4.00e+7 Hz
75 dB

@Frequency 4.00e+7 Hz
With 360° ground termination
Dielectric Strength 177 kV/mm
4500 kV/in
With 360° ground termination
Descriptive Properties Value Comments
Adhesion of Foil to Insulator 4 lbs/in
Adhesion of Sealing adhesive 2.5 lbs/in
Flexibility Pass
IPC-TM-650 Method 2.4.5
Grade Commercial