Material Notes:
Commercial Grade Extruded Elastomer. This is an extruded nickel-plated graphite filled silicone elastomer that provides a minimum shielding effectiveness of 75 dB from 100 MHz to 10 GHz. This low cost, commercial-grade elastomer is suitable for indoor and outdoor applications where excellent resistance to compression set and superior corrosion performance are required.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 70
50 - 70
ASTM D2240
Tensile Strength at Break >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break >= 75 %
>= 75 %
ASTM D412
Compression Set <= 30 %
<= 30 %
ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.50 ohm-cm
<= 0.50 ohm-cm
without pressure-sensitive adhesive; CEPS-0002
<= 1.25 ohm-cm
<= 1.25 ohm-cm
After heat aging; CEPS-0002
Shielding Effectiveness >= 75 dB
>= 75 dB
2 GHz (Plane Wave); MIL-G-83528
>= 75 dB
>= 75 dB
10 GHz (Plane Wave); MIL-G-83528
>= 80 dB
>= 80 dB
100 MHz (E Field); MIL-G-83528
>= 80 dB
>= 80 dB
500 MHz (E Field); MIL-G-83528
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C