Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in salt spray corrosion applications and there are options for addressing fluid immersion requirements as well as Underwriters Laboratories flammability requirements.Extruded onlyInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 64
50 - 64
ASTM D2240
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength 6.130 kN/m
34.98 pli
ASTM D624
Compression Set <= 30 %

@Temperature 100 °C,
Time 252000 sec
<= 30 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flex TR10; ASTM D5470
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Volume Resistivity 0.75 ohm-cm
0.75 ohm-cm
without psa; CEPS-0002
Shielding Effectiveness >= 80 dB

@Frequency 2.00e+9 Hz
>= 80 dB

@Frequency 2.00e+9 Hz
CHO-TM-TP08
>= 80 dB

@Frequency 1.00e+10 Hz
>= 80 dB

@Frequency 1.00e+10 Hz
CHO-TM-TP08
>= 90 dB

@Frequency 1.00e+8 Hz
>= 90 dB

@Frequency 1.00e+8 Hz
CHO-TM-TP08
>= 90 dB

@Frequency 5.00e+8 Hz
>= 90 dB

@Frequency 5.00e+8 Hz
CHO-TM-TP08
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C
Heat Aging <0.85 ohm-cm
150°C for 48 hrs; CEPS-0002