Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Density >= 0.00122 g/cc
>= 0.0000441 lb/in³
Vapor Density
Volatiles <= 50 %
<= 50 %
Vinyl Acetate Content <= 10 %
<= 10 %
Component Elements Properties Metric English Comments
Silver, Ag <= 50 %
<= 50 %
Descriptive Properties Value Comments
Physical Form Silver gray liquid
Toluene wt. % Max 50