Parker Chomerics Tecknit® 72-00015/72-00016 Conductive Silver-Filled Grease

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name Tecknit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit® 72-00015/72-00016 Conductive Silver-Filled Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECKNIT CONDUCTIVE GREASE is a highly conductive silver-filled silicone grease which contains no carbon or graphite. The material will maintain its electrical and lubricating properties over a broad environmental range. These conditions and properties include high and low temperatures, excellent resistance to moisture and humidity, inertness to many chemicals, ozone and radiation. TECKNIT CONDUCTIVE GREASE is a viscous paste which can be applied to vertical or overhead surfaces without dripping or running at elevated operating temperatures.Application Information: TECKNIT CONDUCTIVE GREASE is used on power substation switches and in suspension insulators to reduce EMI noise. It also reduces make-break arcing and pitting of the sliding metal contact surfaces of switches and fills in existing pitted areas with silver/ silicone. In addition, normally closed switches are prevented from sticking due to corrosion or icing. The grease is effective in maintaining a continuous electrical path between contact surfaces which connections of power insulators, which if allowed to arc, can give rise to EMI noise. TECKNIT CONDUCTIVE GREASE is designed to maintain low resistance electrical contact and thereby maintain equipment operation over extended harsh environmental conditions, helping to deliver continuous electrical service.Information provided by Chomerics
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C
374 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.20 ohm-cm
<= 0.20 ohm-cm
QAP-1017
Descriptive Properties Value Comments
Color Silver Gray
Consistency Light Paste
Filler Ag/Glass
Final Condition Non-Setting
Number of Components One
Pot Life Indefinite
at 25°C
Resin Silicone
Shelf Life Unopened Container