Parker Chomerics Tecknit CON/RTV-I One Part: Silver-Filled Silicone RTV

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics Tecknit
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit CON/RTV-I One Part: Silver-Filled Silicone RTV.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECKNIT CON/RTV-I system is a pure silver loaded, one component RTV silicone adhesive sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moisture in the air to form a flexible, resilient, conductive bond or seal.Application Information: TECKNIT CON/RTV-I can be used in the following applications: Bonding or installing various conductive silicone elastomer EMI gaskets. These include silver filled silicone (CONSIL®), silicone filled with stainless steel fiber. (TECKFELT™), silicone impregnated woven (DUOLASTIC™), expanded (TECKSPAN™), metal aluminum wire or silicone filled oriented wire (ELASTOMET®). It can also be used for attaching porous or wire mesh materials.For joining strips of conductive elastomers to form continuous shield/seal rings or gaskets.To form-in-place conductive gasketing to attach shielding windows to frames or bezels, and in turn, installing the framed window on a shielding enclosure; for in place EMI gasketing of shield penetrating components such as connectors or switches: conductively attaching small screens, honeycomb or metal shielding vents to enclosures.For flow-in-place EMI gasketing for grooves in cast boxes or covers or as a conductive seam sealant. Generally, these are field repair or “fix” applications.Information provided by Chomerics
Mechanical Properties Metric English Comments
Shear Strength >= 1.03 MPa
>= 149 psi
Cured; ASTM D1002
Peel Strength >= 0.351 kN/m
>= 2.00 pli
Silicone Aluminum; Cured; ASTM D1876
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Cured
Minimum Service Temperature, Air -59.0 °C
-74.2 °F
Cured
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Cured; QA-1038
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
50%; Recommended for 1/8" dia bead
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
50%; Full Cure
Pot Life 5.0 min

@Temperature 25.0 °C
5.0 min

@Temperature 77.0 °F
Shelf Life 5.50 Month
5.50 Month
Unopened Container
Descriptive Properties Value Comments
Color Silver-Tan
Consistency Thick Paste
Filler Ag
Final Condition Flexible
Number of Components One
Resin Silicone
Volume 1.1 in3
Weight 2 oz