Material Notes:
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is designed to provide reliable cost effective shielding for a wide range of EMI applications. CONSIL-II is manufactured in sheets, molded parts, strips, and die cut flat gaskets.Applications: CONSIL-II should be used where there is a need for high broadband shielding combined with excellent moisture sealing propertiesInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.61 - 2.11 g/cc
1.61 - 2.11 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 80
60 - 80
ASTM D2240
Tensile Strength >= 0.827 MPa
>= 120 psi
ASTM D412
Elongation at Break >= 120 %
>= 120 %
ASTM D412
Tear Strength 7.89 kN/m
45.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.010 ohm-cm
<= 0.010 ohm-cm
Shielding Effectiveness 75 dB

@Frequency 100000 Hz
75 dB

@Frequency 100000 Hz
H-Field
90 dB

@Frequency 1.00e+10 Hz
90 dB

@Frequency 1.00e+10 Hz
Plane Wave
>= 100 dB

@Frequency 1.00e+9 Hz
>= 100 dB

@Frequency 1.00e+9 Hz
Plane Wave
130 dB

@Frequency 1.00e+7 Hz
130 dB

@Frequency 1.00e+7 Hz
E-Field
Descriptive Properties Value Comments
Binder Silicone
Color Tan
Filler Silver-plated glass particles