Material Notes:
Description: CONSIL-N is a silicone elastomer filled with silver-plated nickel particles and designed to provide high shielding effectiveness and corrosion resistance. CONSIL-N is available in sheets and die-cut or molded gaskets.Typical Applications: CONSIL-N is an excellent conductive elastomer for use in applications requiring EMI/EMP shielding and environmental sealing.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.48 - 4.52 g/cc
3.48 - 4.52 g/cc
ASTM D792
Deformation 10 %
10 %
10 pli; 0.125" diameter cord
10 %
10 %
25 pli; 0.125" by 0.25" strip
20 %
20 %
22 pli; 0.125" diameter cord
20 %
20 %
52 pli; 0.125" by 0.25" strip
Mechanical Properties Metric English Comments
Hardness, Shore A 68 - 82
68 - 82
ASTM D2240
Tensile Strength >= 1.38 MPa
>= 200 psi
ASTM D412
Elongation at Break 100 - 300 %
100 - 300 %
ASTM D412
Tear Strength 5.26 kN/m
30.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0050 ohm-cm
<= 0.0050 ohm-cm
Shielding Effectiveness 75 dB

@Frequency 100000 Hz
75 dB

@Frequency 100000 Hz
H-Field
100 dB

@Frequency 1.00e+10 Hz
100 dB

@Frequency 1.00e+10 Hz
Plane Wave
110 dB

@Frequency 1.00e+9 Hz
110 dB

@Frequency 1.00e+9 Hz
Plane Wave
120 dB

@Frequency 1.00e+7 Hz
120 dB

@Frequency 1.00e+7 Hz
E-Field
Descriptive Properties Value Comments
Binder Silicone
Color Gray
Filler Silver Plated Nickel Particles
Users viewing this material also viewed the following: