Material Notes:
Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout industry for seals, gaskets, electrical connectors, electromagnetic shields and other applications subjected to severe operating conditions.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.045 - 3.955 g/cc
3.045 - 3.955 g/cc
ASTM D792
Deformation 10 %
10 %
10 pli; 0.125" diameter cord
10 %
10 %
43 pli; 0.125" by 0.25" strip
20 %
20 %
18 pli; 0.125" diameter cord
20 %
20 %
77 pli; 0.125" by 0.25" strip
Mechanical Properties Metric English Comments
Hardness, Shore A 60 - 70
60 - 70
ASTM D2240
Tensile Strength >= 2.07 MPa
>= 300 psi
ASTM D412
Elongation at Break >= 200 %
>= 200 %
ASTM D412
Tear Strength 7.01 kN/m
40.0 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0020 ohm-cm
<= 0.0020 ohm-cm
Shielding Effectiveness 70 dB

@Frequency 100000 Hz
70 dB

@Frequency 100000 Hz
H-Field
100 dB

@Frequency 1.00e+10 Hz
100 dB

@Frequency 1.00e+10 Hz
Plane Wave
120 dB

@Frequency 1.00e+9 Hz
120 dB

@Frequency 1.00e+9 Hz
Plane Wave
>= 120 dB

@Frequency 1.00e+7 Hz
>= 120 dB

@Frequency 1.00e+7 Hz
E-Field
Descriptive Properties Value Comments
Binder Silicone
Color Red-Brown
Filler Pure Silver
Copyright © lookpolymers.com All Rights Reserved