Parker Chomerics Tecknit Teckfip™ FIP-R Formed in Place Conductive Elastomer

Category Polymer
Manufacturer Parker Chomerics Tecknit
Trade Name Teckfip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics Tecknit Teckfip™ FIP-R Formed in Place Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: FIP-R is based on a very rugged pure silver particle. By using silver as the conductive medium, this compound offers great performance in terms of heat aged electrical conductive stability and prolonged mechanical vibration. In addition to this, the electrical conductivity performance is the highest of all Tecknit FIP compounds.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 2.295 - 3.105 g/cc
2.295 - 3.105 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 43 - 57
43 - 57
Tensile Strength 1.38 MPa
200 psi
Elongation at Break 100 %
100 %
Peel Strength >= 9.00 kN/m
>= 51.4 pli
Compression Set 10 - 25 %
10 - 25 %
28 %

@Temperature 70.0 °C,
Time 79200 sec
28 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.0050 ohm-cm
0.0050 ohm-cm
Surface Resistance 0.015 ohm
0.015 ohm
<= 0.020 ohm

@Temperature 85.0 °C,
Time 605000 sec
<= 0.020 ohm

@Temperature 185 °F,
Time 168 hour
Processing Properties Metric English Comments
Dry Time >= 0.200 hour
>= 0.200 hour
Tack Free
Cure Time <= 1440 min
<= 24.0 hour
Shelf Life 1.00 Month
1.00 Month
Syringe
6.00 Month
6.00 Month
Cartridge
Descriptive Properties Value Comments
Color Pale Yellow
Filler Pure Silver