Material Notes:
Monomer is monochloro para-xylylene. Parylene C is recommended where excellent barrier protection is needed. It can be used up to 125°C where oxygen is present.Parylene is a generic name for poly-para-xylylene polymers used as conformal coatings in protective applications.The coating process exposes objects to the gas-phase monomer at low pressure. Through vacuum deposition, Parylene condenses on the surface in a polycrystalline fashion, providing a coating that is truly conformal and pinhole free.Compared to liquid processes, the effects of gravity and surface tension are negligible -- so there is no bridging, thin-out, pinholes, puddling, run-off or sagging. And, since the process takes place at room temperature, there is no thermal or mechanical stress on the object.Parylene is physically stable and chemically inert within its usable temperature range. Parylene provides excellent protection from moisture, salt spray, corrosive vapors, solvents, airborne contaminants and other hostile environments.Property data obtained following ASTM methods. Information provided by Parylene Coating Services, Inc. (PCS)
Physical Properties Metric English Comments
Density 1.289 g/cc
0.04657 lb/in³
Water Absorption 0.060 %
0.060 %
0.029 inches; 24 hrs.
Moisture Vapor Transmission 0.0551 cc-mm/m²-24hr-atm
0.140 cc-mil/100 in²-24hr-atm
37°C; 90% RH
Oxygen Transmission 2.80 cc-mm/m²-24hr-atm
7.10 cc-mil/100 in²-24hr-atm
23°C
Nitrogen Transmission 0.374 cc-mm/m²-24hr-atm
0.950 cc-mil/100 in²-24hr-atm
23°C
Carbon Dioxide Transmission 3.03 cc-mm/m²-24hr-atm
7.70 cc-mil/100 in²-24hr-atm
23°C
Hydrogen Sulfide Transmission 5.12 cc-mm/m²-24hr-atm
13.0 cc-mil/100 in²-24hr-atm
23°C
Sulfur Dioxide Transmission 4.33 cc-mm/m²-24hr-atm
11.0 cc-mil/100 in²-24hr-atm
23°C
Chlorine Transmission 0.138 cc-mm/m²-24hr-atm
0.350 cc-mil/100 in²-24hr-atm
23°C
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.9 MPa
10000 psi
Tensile Strength, Yield 55.2 MPa
8000 psi
Elongation at Break 200 %
200 %
Elongation at Yield 2.9 %
2.9 %
Tensile Modulus 3.20 GPa
464 ksi
Coefficient of Friction, Dynamic 0.29
0.29
Coefficient of Friction, Static 0.29
0.29
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 20.0 °C
19.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.0820 W/m-K
0.569 BTU-in/hr-ft²-°F
Melting Point 290 °C
554 °F
Maximum Service Temperature, Air 125 °C
257 °F
Continuous
Optical Properties Metric English Comments
Refractive Index 1.639
1.639
Transmission, Visible 90 %
90 %
Optically clear, but reports do not quantify.
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+16 ohm-cm
6.00e+16 ohm-cm
50% RH
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
50% RH
Dielectric Constant 2.95

@Frequency 1e+6 Hz
2.95

@Frequency 1e+6 Hz
3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
3.15

@Frequency 60 Hz
3.15

@Frequency 60 Hz
Dielectric Strength 268 kV/mm
6800 kV/in
Short Time; 1 mil
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
0.019

@Frequency 1000 Hz
0.019

@Frequency 1000 Hz
0.020

@Frequency 60 Hz
0.020

@Frequency 60 Hz
Copyright © lookpolymers.com All Rights Reserved