Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Pasargad Polymer Peyvand
Trade Name Pasadur
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pasargad Polymer Peyvand Pasadur 3P-H8130B PBT, 30% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Polymer Peyvand Co
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ISO 527-2
Elongation at Break 6.0 %
6.0 %
ISO 527-2
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527-2
Charpy Impact Unnotched 5.20 J/cm²
24.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 201 °C
394 °F
Unannealed; ISO 75-2/C
Processing Properties Metric English Comments
Rear Barrel Temperature 260 °C
500 °F
Drying Temperature 60.0 °C
140 °F
Dry Time 1.00 hour
1.00 hour
Descriptive Properties Value Comments
Color Black
Users viewing this material also viewed the following: