Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pau Tai Unistab BC-468A Mixed Metal Liquid Stabilizer for PVC Cadmium/Barium/Zinc Self-Lubricating

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name UNISTAB
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Unistab BC-468A Mixed Metal Liquid Stabilizer for PVC Cadmium/Barium/Zinc Self-Lubricating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is a high-efficiency stabilizer,offering very good early color hold,excellent clarity and long-term heat stability.It is particularly well suited to calendering and extrusion formulations..Information provided by Pau Tai Industrial Corp.