Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 10% Glass Fiber Filled
Manufacturer Penn Fibre Plastics (Ensinger)
Trade Name Pennite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PENNITE® 4512 is a 12% glass fiber reinforced, black pigmented, thermally modified, type 6 nylon, available in sheets and rolls for high performance thermoforming and fabrication applications. PENNITE® 4512 offers an excellent balance of engineering properties combined with a superior melt strength ideally suited to engineered thermoforming products. PENNITE® 4512 exhibits improved strength, stiffness, and creep resistance compared to other nylons used in thermoforming and fabrication. PENNITE® 4512 provides outstanding permeability and chemical resistance to oils, hydrocarbons, and most solvents. PENNITE® 4512 is designed as a cost effective thermoplastic for metal replacement and is ideal for automotive applications such as air ducts, radiator shrouds, fuel cells, covers, structural components and reservoirs.Information provided by Ensinger/PennFibre Plastics, Inc.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 MPa
15900 psi
ASTM D638
115 MPa

@Temperature -40.0 °C
16700 psi

@Temperature -40.0 °F
ASTM D638
Tensile Strength, Ultimate 45.0 MPa

@Temperature 121 °C
6520 psi

@Temperature 250 °F
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
2.0 %

@Temperature -40.0 °C
2.0 %

@Temperature -40.0 °F
ASTM D638
15 %

@Temperature 121 °C
15 %

@Temperature 250 °F
ASTM D638
Flexural Strength 165 MPa
23900 psi
ASTM D790
50.0 MPa

@Temperature 121 °C
7250 psi

@Temperature 250 °F
ASTM D790
200 MPa

@Temperature -40.0 °C
29000 psi

@Temperature -40.0 °F
ASTM D790
Flexural Modulus 4.65 GPa
674 ksi
ASTM D790
0.993 GPa

@Temperature 121 °C
144 ksi

@Temperature 250 °F
ASTM D790
5.20 GPa

@Temperature -40.0 °C
754 ksi

@Temperature -40.0 °F
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
0.374 J/cm

@Temperature -40.0 °C
0.700 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 197 °C
386 °F
ASTM D648
Flammability, UL94 HB
HB