Performance Alloys MoldStar® 90 Copper Mold Alloy

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Performance Alloys
Trade Name MoldStar®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Performance Alloys MoldStar® 90 Copper Mold Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of thermal conductivity, hardness, corrosion resistance and wear.Applications: Mold InsertsThermal PinsMold CoresCavitiesLiftersEtc.Information provided by Performance Alloys.
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 311
311
3000kg
Hardness, Rockwell C 31
31
Tensile Strength at Break 1030 MPa
150000 psi
Tensile Strength, Yield 965 MPa
140000 psi
Elongation at Break 5.0 %
5.0 %
in 2"
Compressive Strength 965 MPa
140000 psi
Thermal Properties Metric English Comments
CTE, linear 17.1 µm/m-°C

@Temperature 20.0 °C
9.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 156 W/m-K

@Temperature 15.6 °C
1080 BTU-in/hr-ft²-°F

@Temperature 60.0 °F
Component Elements Properties Metric English Comments
Copper, Cu 89 %
89 %
Nickel, Ni 7.5 %
7.5 %
Other 3.5 %
3.5 %
Descriptive Properties Value Comments
Thermal diffusivity at 68°F 1.76 ft²/hr