Material Notes:
PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for high speed production lines. Features & Benefits: Ultra-low viscosity Suitable for bonding pre-assembled parts Ideal for close-fitting plastic components Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 2.0 - 3.0 cP

@Temperature 25.0 °C
2.0 - 3.0 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength >= 5.00 MPa
>= 725 psi
PC, Substrate Failure, Shear; ISO 4587
>= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
>= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
7.00 - 9.00 MPa
1020 - 1310 psi
Aluminum, Shear; ISO 4587
8.00 - 10.0 MPa
1160 - 1450 psi
Zinc, Shear; ISO 4587
12.0 - 14.0 MPa
1740 - 2030 psi
Phenolic, Shear; ISO 4587
19.0 - 23.0 MPa
2760 - 3340 psi
Steel, Shear; ISO 4587
Impact 3.0 - 5.0
3.0 - 5.0
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C
180 °F
Minimum Service Temperature, Air -62.2 °C
-80.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 10000 Hz
2.5

@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.0333 - 0.0833 min
0.000556 - 0.00139 hour
Buna N Rubber, handling time
0.0500 - 0.0833 min
0.000833 - 0.00139 hour
Steel, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
Phenolic, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.05
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C