Material Notes:
PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding dissimilar materials which could be subject to thermal shock or thermal cycling. 2050 is ideal for use on flexible or semiporous surfaces. It can also be used to bond silicone when used in conjunction with Permabond Polyolefin Primer (POP). Features & Benefits: Medium-high viscosity Flexible and toughened Fast cure Easy to apply and dispense 100% reactive, no solvents Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 1200 - 1800 cP

@Temperature 25.0 °C
1200 - 1800 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ISO 868
Adhesive Bond Strength >= 5.00 MPa
>= 725 psi
PC, Substrate Failure, Shear; ISO 4587
>= 6.00 MPa
>= 870 psi
ABS, Substrate Failure, Shear; ISO 4587
>= 6.00 MPa
>= 870 psi
PVC, Substrate Failure, Shear; ISO 4587
16.0 - 20.0 MPa
2320 - 2900 psi
Steel, Shear; ISO 4587
Impact 5.0 - 10
5.0 - 10
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 2.5

@Frequency 10000 Hz
2.5

@Frequency 10000 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.167 min
0.00139 - 0.00278 hour
Buna N Rubber, handling time
0.0833 - 0.167 min
0.00139 - 0.00278 hour
PVC, handling time
0.167 - 0.250 min
0.00278 - 0.00417 hour
Steel, handling time
1440 min
24.0 hour
full strength
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.2
Strength Retention 10% at 150°C
Relative to 0°C
100% at 0°C
Relative to 0°C
30% at 100°C
Relative to 0°C
55% at -50°C
Relative to 0°C
90% at 50°C
Relative to 0°C