Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond A126 Anaerobic Retainer

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond A126 Anaerobic Retainer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for use on tight fitting components or where the adhesive needs to be applied after assembly. In addition it may also be used to seal porosity in welds or castings. Features & Benefits Vibration resistant Can be applied post-assembly Improved fatigue life Seals porosity in welds and castings WRAS listed for contact with wholesome (potable) water Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Uncured
Viscosity 10 - 30 cP

@Temperature 25.0 °C
10 - 30 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 10.0 - 20.0 MPa
1450 - 2900 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, working strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Zinc, handling strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
M10 steel, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Zinc, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance Green
Uncured
Maximum Gap Fill (mm) 0.05
Maximum Thread Size M10
Strength Retention 50% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 14
M10 steel, break
34
M10 steel, prevail
UV Fluorescence Yes
Uncured
Users viewing this material also viewed the following: