Material Notes:
Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel and tapered threads, the delayed cure allows accurate alignment of components. Capable of giving an instant pressure seal and not drying out like many mastics, re-work can effectively be eliminated. Should disassembly be necessary, this can be accomplished using normal tools. Features & Benefits Allows alignment of parts during cure No loose particles to clog valves Instant low pressure seal Excellent chemical resistance KIWA approved WRAS listed for contact with wholesome (potable) water Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 6000 cP

@Temperature 25.0 °C
6000 cP

@Temperature 77.0 °F
at 20 rpm vibration
40000 cP

@Temperature 25.0 °C
40000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 6.00 MPa
870 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 7.02 min

@Temperature 23.0 °C
0.117 hour

@Temperature 73.4 °F
Brass, handling strength
45.0 min

@Temperature 23.0 °C
0.750 hour

@Temperature 73.4 °F
M10 steel, handling strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Brass, working strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Zinc, handling strength
120 min

@Temperature 23.0 °C
2.00 hour

@Temperature 73.4 °F
M10 steel, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Zinc, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance White
Uncured
Maximum Gap Fill (mm) 0.5
Maximum Thread Size M56
Strength Retention 20% at 150°C
Relative to 0°C
70% at 100°C
Relative to 0°C
90% at 50°C
Relative to 0°C
Torque Strength (N m) 10
M10 steel, break
7
M10 steel, prevail
UV Fluorescence Yes