PERMABOND® ES578 is a single-part heat cured epoxy adhesive with excellent adhesion to metal surfaces, ceramics as well as composite materials. ES578 provides excellent thermal conductivity and bond strength. ES578 was designed for application requiring heat dissipation such as bonding aluminum heat sinks to ceramic headers. The cured adhesive has been designed to meet the fire retardancy requirements of UL94 V-0. Features & Benefits: Very good thermal conductivity Excellent resistance to vibration Easy to use – no mixing required High shear and peel strength High temperature resistance Good resistance to chemicals Designed to meet the requirements of UL94 Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.55 g/cc
1.55 g/cc
Uncured
Viscosity 600000 - 800000 cP

@Temperature 25.0 °C
600000 - 800000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 84
84
Adhesive Bond Strength 14.0 - 27.0 MPa
2030 - 3920 psi
Zinc, Shear; ASTM D1002
17.0 - 31.0 MPa
2470 - 4500 psi
Aluminum, Shear; ASTM D1002
27.0 - 41.0 MPa
3920 - 5950 psi
Steel, Shear; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C
25.0 µin/in-°F
Thermal Conductivity 1.30 W/m-K
9.02 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Cure Time <= 3.00 min
<= 0.0500 hour
Induction
30.0 min

@Temperature 150 °C
0.500 hour

@Temperature 302 °F
Oven
60.0 min

@Temperature 130 °C
1.00 hour

@Temperature 266 °F
Oven
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Black
Uncured
Maximum Gap Fill (mm) 5
Strength Retention 100% at 0°C
Relative to 0°C
25% at 200°C
Relative to 0°C
65% at 150°C