Material Notes:
Permabond® LH050 pipe sealant with PTFE is a general purpose pipe sealant that provides instant air pressure seal up to 1000 psi with limited hand tightening. After cure, the sealing capability is typically up to the burst rating of the pipe itself. The low locking strength allows easy disassembly. Permabond® LH050 pipe sealant performs well on most metals, particularly steel and brass. It provides an excellent alternative to pipe dopes and pipe tapes for sealing pipe joints. It cures anaerobically when in contact with metal parts (as in a threaded pipe joint). When applied, LH050 dispenses as a smooth paste, filling the entire space between the threaded parts. It then cures at ambient temperature to form a solid plastic, completely sealing against hydraulic fluids, air, gases and chemicals. In addition, it locks the pipes, plugs or fittings against vibration loosening, tampering and variable temperature effects. Features & Benefits: Full cure seal to the burst rating of pipeEasy to use and apply Directional freedom Does not contain solvents Excellent chemical and temperature resistance Cures at room temperature Will not shred, tear or cause blockages Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 250000 cP

@Temperature 25.0 °C
250000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 7.00 MPa
1020 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, handling strength
120 min

@Temperature 23.0 °C
2.00 hour

@Temperature 73.4 °F
M10 steel, handling strength
180 min

@Temperature 23.0 °C
3.00 hour

@Temperature 73.4 °F
Zinc, handling strength
180 - 360 min

@Temperature 23.0 °C
3.00 - 6.00 hour

@Temperature 73.4 °F
Brass, working strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
Stainless steel, handling strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
M10 steel, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Zinc, working strength
4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 20% at 200°C
Relative to 0°C
60% at 150°C
Relative to 0°C
85% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 3
M10 steel, prevail
4
M10 steel, break
UV Fluorescence No
Uncured