Permabond LM113 Anaerobic Threadlocker

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond LM113 Anaerobic Threadlocker.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotropic viscosity, the liquid adhesive will not run away from the area of application. Permabond LM113 Threadlocker cures reliably and fast on steel, cadmium, zinc and other plated fasteners. Features & Benefits: Prevents vibration loosening Controlled off-torque Full cure at room temperature Low strength for easy disassembly Lubricates threads for easier assembly Provides corrosion protection Superior environmental resistance Environmentally friendly – 100% solids Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 1200 cP

@Temperature 25.0 °C
1200 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.00 MPa
725 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 7.02 min

@Temperature 23.0 °C
0.117 hour

@Temperature 73.4 °F
Brass, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Brass, working strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Zinc, handling strength
360 min

@Temperature 23.0 °C
6.00 hour

@Temperature 73.4 °F
M10 steel, working strength
4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
M10 steel, full strength
4320 min

@Temperature 23.0 °C
72.0 hour

@Temperature 73.4 °F
Zinc, working strength
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Purple
Uncured
Maximum Gap Fill (mm) 0.15
Maximum Thread Size M20
Strength Retention 20% at 150°C
Relative to 0°C
70% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 5
M10 steel, prevail
9
M10 steel, break