Material Notes:
PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is convenient to use in an easy-to-dispense cartridge or it can be used bead on bead without a mixing nozzle. Features & Benefits: Adhesion to a wide variety of substrates Fast cure at room temperature Can be used with or without nozzle High shear and peel strength Good impact strength Good chemical resistance Information provided by Permabond.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
TA4302B
1.05 g/cc
0.0379 lb/in³
TA4302A
Viscosity 4000 - 5000 cP

@Temperature 25.0 °C
4000 - 5000 cP

@Temperature 77.0 °F
TA4302A
4000 - 5000 cP

@Temperature 25.0 °C
4000 - 5000 cP

@Temperature 77.0 °F
TA4302B
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Tensile Strength 30.0 MPa
4350 psi
DIN 53288
Adhesive Bond Strength 22.0 - 25.0 MPa
3190 - 3630 psi
Mild steel, Shear
Peel Strength 3.00 - 4.80 kN/m
17.1 - 27.4 pli
ISO 4578
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ASTM D696
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.6

@Frequency 1.00e+7 Hz
4.6

@Frequency 1.00e+7 Hz
ASTM D150
Dielectric Strength 30.0 - 50.0 kV/mm
762 - 1270 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 3.00 - 5.00 min
0.0500 - 0.0833 hour
handling time
15.0 - 30.0 min
0.250 - 0.500 hour
working strength
1440 min
24.0 hour
full cure
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Green, TA4302B
Uncured
Pink, TA4302A
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 100% at 0°C
Relative to 0°C
15% at 175°C
Relative to 0°C
22% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
96% at 50°C
Relative to 0°C