Material Notes:
PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength 1-3 minutes when the adhesive and the Initiator 43 come in contact. Permabond TA436 offers high shear and impact resistant bonds and improved high temperature resistance. Features & Benefits: Adhesion to a wide variety of substrates Fast cure at room temperature No mix application High shear and peel strength Good impact strength High temperature resistance Information provided by Permabond.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
uncured
Viscosity 16000 - 18000 cP

@Temperature 25.0 °C
16000 - 18000 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Tensile Strength 25.0 MPa
3630 psi
DIN 53288
Adhesive Bond Strength 15.0 - 25.0 MPa
2180 - 3630 psi
Mild steel, Shear
Impact 25
25
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Peel Strength 1.80 - 2.60 kN/m
10.3 - 14.8 pli
ISO 4578
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ASTM D696
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
ASTM C177
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Dielectric Constant 4.6

@Frequency 1.00e+7 Hz
4.6

@Frequency 1.00e+7 Hz
ASTM D150
Dielectric Strength 30.0 - 50.0 kV/mm
762 - 1270 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
handling time
30.0 - 60.0 min
0.500 - 1.00 hour
working strength
1440 min
24.0 hour
full cure
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Amber liquid
Uncured
Maximum Gap Fill (mm) 0.5
Strength Retention 100% at 0°C
Relative to 0°C
15% at 175°C
Relative to 0°C
22% at 150°C
Relative to 0°C
75% at 100°C
Relative to 0°C
96% at 50°C
Relative to 0°C
Copyright © lookpolymers.com All Rights Reserved