Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Perstorp Compounds AMITEC VXO UF/MF blend

Category Polymer , Thermoset , Melamine
Manufacturer Perstorp Compounds
Trade Name AMITEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Perstorp Compounds AMITEC VXO UF/MF blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A special Urea Formaldehyde/Melamine Formaldehyde blend that enhances surface properties and is optimized for cost-effective injection molding of visible components.Information provided by Perstorp Compounds Inc.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.0090 cm/cm
0.0070 - 0.0090 in/in
DIN 53 464
Mechanical Properties Metric English Comments
Elongation at Break 2.4 %
2.4 %
ISO 178
Flexural Strength >= 130 MPa
>= 18900 psi
ISO 178
Charpy Impact Unnotched >= 1.40 J/cm²
>= 6.66 ft-lb/in²
ISO 179
Charpy Impact, Notched >= 0.140 J/cm²
>= 0.666 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 160 °C
>= 320 °F
ISO 175
Deflection Temperature at 8.0 MPa >= 100 °C
>= 212 °F
ISO 175
Flammability, UL94 V-0
V-0
Shrinkage 0.80 - 1.1 %
0.80 - 1.1 %
Post Shrinkage; DIN 53 464
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DIN 53 483
Surface Resistance >= 1.00e+10 ohm
>= 1.00e+10 ohm
DIN 53 482
Dielectric Constant 5.0
5.0
DIN 53 483
Dissipation Factor <= 0.10

@Frequency 1000 Hz
<= 0.10

@Frequency 1000 Hz
tan delta; DIN 53 483
Comparative Tracking Index >= 600 V
>= 600 V
IEC 112
Descriptive Properties Value Comments
Glow Bar 960°C 180 sec BH2-8
IEC 707
Water Absorption [mg] <200
DIN 53 495/23°C 96h
Users viewing this material also viewed the following: