Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Perstorp Compounds Aminel FX Melamine

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Melamine , Melamine Formaldehyde, Molded, Cellulose Filler
Manufacturer Perstorp Compounds
Trade Name Aminel
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Perstorp Compounds Aminel FX Melamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp Compounds Inc.
Physical Properties Metric English Comments
Bulk Density 0.600 - 0.700 g/cc
0.0217 - 0.0253 lb/in³
DIN 53 468
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
DIN 53 464
Mechanical Properties Metric English Comments
Tensile Strength at Break 75.0 MPa
10900 psi
ISO 178
Elongation at Break 2.0 %
2.0 %
ISO 178
Tensile Modulus 3.00 GPa
435 ksi
ISO 527
Flexural Strength 125 MPa
18100 psi
ISO 178
Flexural Modulus 5.50 - 6.50 GPa
798 - 943 ksi
ISO 178
Compressive Strength 210 - 240 MPa
30500 - 34800 psi
ISO 604
Charpy Impact Unnotched 1.60 - 1.80 J/cm²
7.61 - 8.57 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Thermal Conductivity 0.258 W/m-K
1.79 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
ISO 175
Deflection Temperature at 8.0 MPa 110 °C
230 °F
ISO 175
Flammability, UL94 V-0
V-0
Oxygen Index >= 30 %
>= 30 %
ASTM D2863
Shrinkage 1.30 - 1.60 %

@Temperature 110 °C,
Time 605000 sec
1.30 - 1.60 %

@Temperature 230 °F,
Time 168 hour
Post Shrinkage; DIN 53 464
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
DIN 53 483
Surface Resistance >= 1.00e+11 ohm
>= 1.00e+11 ohm
DIN 53 482
Dielectric Constant 6.0 - 7.0
6.0 - 7.0
DIN 53 483
Dissipation Factor 0.050

@Frequency 1000 Hz
0.050

@Frequency 1000 Hz
tan delta; DIN 53 483
Arc Resistance >= 120 sec
>= 120 sec
Comparative Tracking Index >= 600 V
>= 600 V
IEC 112
Descriptive Properties Value Comments
Glow Bar 960°C 180 sec BH2-8
IEC 707
Water Absorption [mg] <200
DIN 53 495/23°C 96h
Users viewing this material also viewed the following: